[ad_1]
Chilly Traits
Constant shade.
Working Notes
Coloration normally deepens on firing. Attainable darkish interface response with selenium and/or sulfur glasses (000137, 001122, 001125, 000124, 000125, 001137, 001437). Much less viscous (softer) than most different glasses. Some gold-bearing putting glasses, like this one, must be fired with a 2 hour maintain at 1225°F through the preliminary levels of the firing cycle. If fired with out this maintain, they might not strike in any respect, or they might strike however seem spotty and have a blue-brown solid, versus the specified goal shade. This full-fuse schedule successfully strikes these glasses:
RATE | TEMPERATURE | HOLD TIME |
---|---|---|
* | 1225ºF | 2:00 |
600ºF | 1490 | 0:10 |
9999 | 900 | ** |
**The rest of cycle depends upon the thickness of the piece. Seek the advice of the Bullseye Annealing Chart. For color-sensitive initiatives, we suggest testing the cycle you intend to make use of by fusing a small pattern of an analogous setup in the identical kiln because the undertaking to finest predict last shade outcomes.
[ad_2]